Coagulation of fines in fluorite froth flotation
- Autores
- Sarquis, Pedro Edgardo; Gonzalez, Mercedes Isabel; Moyano, Silvia Adriana; Bazan Brizuela, Vanesa Lucia
- Año de publicación
- 2011
- Idioma
- español castellano
- Tipo de recurso
- artículo
- Estado
- versión publicada
- Descripción
- Fluorite, a valuable mineral in the metallurgical industry, can be found together with silicates, carbonates and oxides in ore deposits. Commercial concentrates with more than 95 % of CaF2 are obtained processing the mineral in flotation plants and using oleic acid as fluorite collector. Depressor reagents such as sodium silicate, tannin and sodium carbonate are commonly employed to allow the oleic acid selective performance. These reagents cause a dispersant effect separating the solid-liquid solution on tailing plants. Fine particles in the recovered water enter the circuit and affect the flotation efficiency. The effect of coagulant ions was studied as a method to clarify the returned water. The problem of the presence of these ions is related to its reactions with the collector by the formation of compounds and possibly on the selectivity. Variable quantities of Al3+, Fe3+ and Ca2+ ions were added to the flotation to evaluate its effect on the fluorite recovery, in the selectivity and in solids content in recirculation water. Results show that some ions fail to improve water quality and are detrimental to flotation. On the contrary, some ions contribute to reduce fine content in suspension. Therefore, although there is a recovery reduction, such effect can be counteracted increasing the collector consumption a little.
La fluorita es un mineral de mucha importancia en la industria metalúrgica. Se presenta acompañada de silicatos, carbonatos y óxidos. Para la obtención de concentrados comerciales, más de 95 % de CaF2, el mineral se procesa en plantas de flotación donde se usa ácido oleico como colector de la fluorita. Para que el ácido oleico actúe electivamente es común el uso de reactivos depresores: silicato de sodio, tanino y carbonato de sodio. Estos agentes tienen un efecto dispersante que se evidencia en la separación de sólido-llquido sobre las colas de las plantas. El agua recuperada contiene finos que al ingresar al circuito afectan notoriamente la eficiencia de la flotación. Se estudió el efecto de iones coagulantes para clarificar el agua de retorno. El problema de estos iones está relacionado con sus reacciones con el colector por la fonnación de compuestos y, posiblemente, sobre la selectividad. Se agregaron cantidades variables de iones Al3+, Fe3++ y Ca2+ y se evaluó la recuperación de fluorita, la selectividad y en el contenido de sólidos en el agua de los efluentes. Los resultados muestran que algunos iones no solamente no mejoran la calidad del agua sino que además son perjudiciales en la flotación. Otros, por el contrarío, contribuyen a reducir el contenido de finos en suspensión. Por lo tanto, y si bien hay una pérdida en la recuperación, este efecto se puede contrarrestar con un pequeño aumento en el consumo de colector
Fil: Sarquis, Pedro Edgardo. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina
Fil: Gonzalez, Mercedes Isabel. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - San Juan; Argentina
Fil: Moyano, Silvia Adriana. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina
Fil: Bazan Brizuela, Vanesa Lucia. Consejo Nacional de Investigaciones Científicas y Técnicas; Argentina. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina - Materia
-
COAGULATION
FLOTATION
FLUORITE
REAGENTS
SLIMES - Nivel de accesibilidad
- acceso abierto
- Condiciones de uso
- https://creativecommons.org/licenses/by-nc-sa/2.5/ar/
- Repositorio
- Institución
- Consejo Nacional de Investigaciones Científicas y Técnicas
- OAI Identificador
- oai:ri.conicet.gov.ar:11336/199033
Ver los metadatos del registro completo
id |
CONICETDig_0ffd322c5171acd72accdf516e6eecd3 |
---|---|
oai_identifier_str |
oai:ri.conicet.gov.ar:11336/199033 |
network_acronym_str |
CONICETDig |
repository_id_str |
3498 |
network_name_str |
CONICET Digital (CONICET) |
spelling |
Coagulation of fines in fluorite froth flotationCoagulación de finos en la flotación de la fluoritaSarquis, Pedro EdgardoGonzalez, Mercedes IsabelMoyano, Silvia AdrianaBazan Brizuela, Vanesa LuciaCOAGULATIONFLOTATIONFLUORITEREAGENTSSLIMEShttps://purl.org/becyt/ford/2.4https://purl.org/becyt/ford/2Fluorite, a valuable mineral in the metallurgical industry, can be found together with silicates, carbonates and oxides in ore deposits. Commercial concentrates with more than 95 % of CaF2 are obtained processing the mineral in flotation plants and using oleic acid as fluorite collector. Depressor reagents such as sodium silicate, tannin and sodium carbonate are commonly employed to allow the oleic acid selective performance. These reagents cause a dispersant effect separating the solid-liquid solution on tailing plants. Fine particles in the recovered water enter the circuit and affect the flotation efficiency. The effect of coagulant ions was studied as a method to clarify the returned water. The problem of the presence of these ions is related to its reactions with the collector by the formation of compounds and possibly on the selectivity. Variable quantities of Al3+, Fe3+ and Ca2+ ions were added to the flotation to evaluate its effect on the fluorite recovery, in the selectivity and in solids content in recirculation water. Results show that some ions fail to improve water quality and are detrimental to flotation. On the contrary, some ions contribute to reduce fine content in suspension. Therefore, although there is a recovery reduction, such effect can be counteracted increasing the collector consumption a little.La fluorita es un mineral de mucha importancia en la industria metalúrgica. Se presenta acompañada de silicatos, carbonatos y óxidos. Para la obtención de concentrados comerciales, más de 95 % de CaF2, el mineral se procesa en plantas de flotación donde se usa ácido oleico como colector de la fluorita. Para que el ácido oleico actúe electivamente es común el uso de reactivos depresores: silicato de sodio, tanino y carbonato de sodio. Estos agentes tienen un efecto dispersante que se evidencia en la separación de sólido-llquido sobre las colas de las plantas. El agua recuperada contiene finos que al ingresar al circuito afectan notoriamente la eficiencia de la flotación. Se estudió el efecto de iones coagulantes para clarificar el agua de retorno. El problema de estos iones está relacionado con sus reacciones con el colector por la fonnación de compuestos y, posiblemente, sobre la selectividad. Se agregaron cantidades variables de iones Al3+, Fe3++ y Ca2+ y se evaluó la recuperación de fluorita, la selectividad y en el contenido de sólidos en el agua de los efluentes. Los resultados muestran que algunos iones no solamente no mejoran la calidad del agua sino que además son perjudiciales en la flotación. Otros, por el contrarío, contribuyen a reducir el contenido de finos en suspensión. Por lo tanto, y si bien hay una pérdida en la recuperación, este efecto se puede contrarrestar con un pequeño aumento en el consumo de colectorFil: Sarquis, Pedro Edgardo. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; ArgentinaFil: Gonzalez, Mercedes Isabel. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - San Juan; ArgentinaFil: Moyano, Silvia Adriana. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; ArgentinaFil: Bazan Brizuela, Vanesa Lucia. Consejo Nacional de Investigaciones Científicas y Técnicas; Argentina. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; ArgentinaCentro de Investigaciones Metalúrgicas2011-05info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionhttp://purl.org/coar/resource_type/c_6501info:ar-repo/semantics/articuloapplication/pdfapplication/pdfapplication/pdfapplication/pdfhttp://hdl.handle.net/11336/199033Sarquis, Pedro Edgardo; Gonzalez, Mercedes Isabel; Moyano, Silvia Adriana; Bazan Brizuela, Vanesa Lucia; Coagulation of fines in fluorite froth flotation; Centro de Investigaciones Metalúrgicas; Revista de Metalurgia; 47; 3; 5-2011; 205-2110034-85701988-4222CONICET DigitalCONICETspainfo:eu-repo/semantics/altIdentifier/url/https://revistademetalurgia.revistas.csic.es/index.php/revistademetalurgia/article/view/1191info:eu-repo/semantics/altIdentifier/url/https://dialnet.unirioja.es/servlet/articulo?codigo=3695547info:eu-repo/semantics/altIdentifier/doi/10.3989/revmetalm.1037info:eu-repo/semantics/openAccesshttps://creativecommons.org/licenses/by-nc-sa/2.5/ar/reponame:CONICET Digital (CONICET)instname:Consejo Nacional de Investigaciones Científicas y Técnicas2025-09-29T09:37:06Zoai:ri.conicet.gov.ar:11336/199033instacron:CONICETInstitucionalhttp://ri.conicet.gov.ar/Organismo científico-tecnológicoNo correspondehttp://ri.conicet.gov.ar/oai/requestdasensio@conicet.gov.ar; lcarlino@conicet.gov.arArgentinaNo correspondeNo correspondeNo correspondeopendoar:34982025-09-29 09:37:07.182CONICET Digital (CONICET) - Consejo Nacional de Investigaciones Científicas y Técnicasfalse |
dc.title.none.fl_str_mv |
Coagulation of fines in fluorite froth flotation Coagulación de finos en la flotación de la fluorita |
title |
Coagulation of fines in fluorite froth flotation |
spellingShingle |
Coagulation of fines in fluorite froth flotation Sarquis, Pedro Edgardo COAGULATION FLOTATION FLUORITE REAGENTS SLIMES |
title_short |
Coagulation of fines in fluorite froth flotation |
title_full |
Coagulation of fines in fluorite froth flotation |
title_fullStr |
Coagulation of fines in fluorite froth flotation |
title_full_unstemmed |
Coagulation of fines in fluorite froth flotation |
title_sort |
Coagulation of fines in fluorite froth flotation |
dc.creator.none.fl_str_mv |
Sarquis, Pedro Edgardo Gonzalez, Mercedes Isabel Moyano, Silvia Adriana Bazan Brizuela, Vanesa Lucia |
author |
Sarquis, Pedro Edgardo |
author_facet |
Sarquis, Pedro Edgardo Gonzalez, Mercedes Isabel Moyano, Silvia Adriana Bazan Brizuela, Vanesa Lucia |
author_role |
author |
author2 |
Gonzalez, Mercedes Isabel Moyano, Silvia Adriana Bazan Brizuela, Vanesa Lucia |
author2_role |
author author author |
dc.subject.none.fl_str_mv |
COAGULATION FLOTATION FLUORITE REAGENTS SLIMES |
topic |
COAGULATION FLOTATION FLUORITE REAGENTS SLIMES |
purl_subject.fl_str_mv |
https://purl.org/becyt/ford/2.4 https://purl.org/becyt/ford/2 |
dc.description.none.fl_txt_mv |
Fluorite, a valuable mineral in the metallurgical industry, can be found together with silicates, carbonates and oxides in ore deposits. Commercial concentrates with more than 95 % of CaF2 are obtained processing the mineral in flotation plants and using oleic acid as fluorite collector. Depressor reagents such as sodium silicate, tannin and sodium carbonate are commonly employed to allow the oleic acid selective performance. These reagents cause a dispersant effect separating the solid-liquid solution on tailing plants. Fine particles in the recovered water enter the circuit and affect the flotation efficiency. The effect of coagulant ions was studied as a method to clarify the returned water. The problem of the presence of these ions is related to its reactions with the collector by the formation of compounds and possibly on the selectivity. Variable quantities of Al3+, Fe3+ and Ca2+ ions were added to the flotation to evaluate its effect on the fluorite recovery, in the selectivity and in solids content in recirculation water. Results show that some ions fail to improve water quality and are detrimental to flotation. On the contrary, some ions contribute to reduce fine content in suspension. Therefore, although there is a recovery reduction, such effect can be counteracted increasing the collector consumption a little. La fluorita es un mineral de mucha importancia en la industria metalúrgica. Se presenta acompañada de silicatos, carbonatos y óxidos. Para la obtención de concentrados comerciales, más de 95 % de CaF2, el mineral se procesa en plantas de flotación donde se usa ácido oleico como colector de la fluorita. Para que el ácido oleico actúe electivamente es común el uso de reactivos depresores: silicato de sodio, tanino y carbonato de sodio. Estos agentes tienen un efecto dispersante que se evidencia en la separación de sólido-llquido sobre las colas de las plantas. El agua recuperada contiene finos que al ingresar al circuito afectan notoriamente la eficiencia de la flotación. Se estudió el efecto de iones coagulantes para clarificar el agua de retorno. El problema de estos iones está relacionado con sus reacciones con el colector por la fonnación de compuestos y, posiblemente, sobre la selectividad. Se agregaron cantidades variables de iones Al3+, Fe3++ y Ca2+ y se evaluó la recuperación de fluorita, la selectividad y en el contenido de sólidos en el agua de los efluentes. Los resultados muestran que algunos iones no solamente no mejoran la calidad del agua sino que además son perjudiciales en la flotación. Otros, por el contrarío, contribuyen a reducir el contenido de finos en suspensión. Por lo tanto, y si bien hay una pérdida en la recuperación, este efecto se puede contrarrestar con un pequeño aumento en el consumo de colector Fil: Sarquis, Pedro Edgardo. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina Fil: Gonzalez, Mercedes Isabel. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - San Juan; Argentina Fil: Moyano, Silvia Adriana. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina Fil: Bazan Brizuela, Vanesa Lucia. Consejo Nacional de Investigaciones Científicas y Técnicas; Argentina. Universidad Nacional de San Juan. Facultad de Ingeniería. Instituto de Investigaciones Mineras; Argentina |
description |
Fluorite, a valuable mineral in the metallurgical industry, can be found together with silicates, carbonates and oxides in ore deposits. Commercial concentrates with more than 95 % of CaF2 are obtained processing the mineral in flotation plants and using oleic acid as fluorite collector. Depressor reagents such as sodium silicate, tannin and sodium carbonate are commonly employed to allow the oleic acid selective performance. These reagents cause a dispersant effect separating the solid-liquid solution on tailing plants. Fine particles in the recovered water enter the circuit and affect the flotation efficiency. The effect of coagulant ions was studied as a method to clarify the returned water. The problem of the presence of these ions is related to its reactions with the collector by the formation of compounds and possibly on the selectivity. Variable quantities of Al3+, Fe3+ and Ca2+ ions were added to the flotation to evaluate its effect on the fluorite recovery, in the selectivity and in solids content in recirculation water. Results show that some ions fail to improve water quality and are detrimental to flotation. On the contrary, some ions contribute to reduce fine content in suspension. Therefore, although there is a recovery reduction, such effect can be counteracted increasing the collector consumption a little. |
publishDate |
2011 |
dc.date.none.fl_str_mv |
2011-05 |
dc.type.none.fl_str_mv |
info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion http://purl.org/coar/resource_type/c_6501 info:ar-repo/semantics/articulo |
format |
article |
status_str |
publishedVersion |
dc.identifier.none.fl_str_mv |
http://hdl.handle.net/11336/199033 Sarquis, Pedro Edgardo; Gonzalez, Mercedes Isabel; Moyano, Silvia Adriana; Bazan Brizuela, Vanesa Lucia; Coagulation of fines in fluorite froth flotation; Centro de Investigaciones Metalúrgicas; Revista de Metalurgia; 47; 3; 5-2011; 205-211 0034-8570 1988-4222 CONICET Digital CONICET |
url |
http://hdl.handle.net/11336/199033 |
identifier_str_mv |
Sarquis, Pedro Edgardo; Gonzalez, Mercedes Isabel; Moyano, Silvia Adriana; Bazan Brizuela, Vanesa Lucia; Coagulation of fines in fluorite froth flotation; Centro de Investigaciones Metalúrgicas; Revista de Metalurgia; 47; 3; 5-2011; 205-211 0034-8570 1988-4222 CONICET Digital CONICET |
dc.language.none.fl_str_mv |
spa |
language |
spa |
dc.relation.none.fl_str_mv |
info:eu-repo/semantics/altIdentifier/url/https://revistademetalurgia.revistas.csic.es/index.php/revistademetalurgia/article/view/1191 info:eu-repo/semantics/altIdentifier/url/https://dialnet.unirioja.es/servlet/articulo?codigo=3695547 info:eu-repo/semantics/altIdentifier/doi/10.3989/revmetalm.1037 |
dc.rights.none.fl_str_mv |
info:eu-repo/semantics/openAccess https://creativecommons.org/licenses/by-nc-sa/2.5/ar/ |
eu_rights_str_mv |
openAccess |
rights_invalid_str_mv |
https://creativecommons.org/licenses/by-nc-sa/2.5/ar/ |
dc.format.none.fl_str_mv |
application/pdf application/pdf application/pdf application/pdf |
dc.publisher.none.fl_str_mv |
Centro de Investigaciones Metalúrgicas |
publisher.none.fl_str_mv |
Centro de Investigaciones Metalúrgicas |
dc.source.none.fl_str_mv |
reponame:CONICET Digital (CONICET) instname:Consejo Nacional de Investigaciones Científicas y Técnicas |
reponame_str |
CONICET Digital (CONICET) |
collection |
CONICET Digital (CONICET) |
instname_str |
Consejo Nacional de Investigaciones Científicas y Técnicas |
repository.name.fl_str_mv |
CONICET Digital (CONICET) - Consejo Nacional de Investigaciones Científicas y Técnicas |
repository.mail.fl_str_mv |
dasensio@conicet.gov.ar; lcarlino@conicet.gov.ar |
_version_ |
1844613168091889664 |
score |
13.070432 |