Antifouling Paints with Zinc “Tannate”
- Autores
- Bellotti, Natalia; Deyá, Marta Cecilia; Del Amo, Delia Beatriz; Romagnoli, Roberto
- Año de publicación
- 2010
- Idioma
- inglés
- Tipo de recurso
- artículo
- Estado
- versión publicada
- Descripción
- During the past decade, the necessity of new ecofriendly antifouling pigments was established. Among these new pigments, special attention should be paid to tannin and its derivatives. Tannins are synthesized by plants as part of their defense mechanism against the attack of pathogens. The objective of this work was to study the antifouling efficiency of paints containing zinc “tannate” in artificial seawater. The zinc “tannate” was precipitated at pH 4 and pH 8. Insoluble and soluble matrix antifouling paints, with different plasticizers, were formulated and tannins leached from the paints immersed in artificial seawater were determined by the Folin-Denis assay for polyphenols. The antifouling action of paints was assessed in a natural seawater environment. The results showed that the leaching rate of tannin from insoluble matrix paint decreases, reaching a constant value after 25 days of immersion. In the case of the soluble matrix paints, a lesser amount of tannin was leached, depending on the tannin and the plasticizer employed. The results in a natural sea environment are dependent on the matrix and the plasticizer employed.
Centro de Investigación y Desarrollo en Tecnología de Pinturas - Materia
-
Ingeniería Química
Antifouling
Tannin
Paints - Nivel de accesibilidad
- acceso abierto
- Condiciones de uso
- http://creativecommons.org/licenses/by-nc-nd/4.0/
- Repositorio
- Institución
- Universidad Nacional de La Plata
- OAI Identificador
- oai:sedici.unlp.edu.ar:10915/94523
Ver los metadatos del registro completo
id |
SEDICI_d04e63231978cdff83ab7c6ee23992da |
---|---|
oai_identifier_str |
oai:sedici.unlp.edu.ar:10915/94523 |
network_acronym_str |
SEDICI |
repository_id_str |
1329 |
network_name_str |
SEDICI (UNLP) |
spelling |
Antifouling Paints with Zinc “Tannate”Bellotti, NataliaDeyá, Marta CeciliaDel Amo, Delia BeatrizRomagnoli, RobertoIngeniería QuímicaAntifoulingTanninPaintsDuring the past decade, the necessity of new ecofriendly antifouling pigments was established. Among these new pigments, special attention should be paid to tannin and its derivatives. Tannins are synthesized by plants as part of their defense mechanism against the attack of pathogens. The objective of this work was to study the antifouling efficiency of paints containing zinc “tannate” in artificial seawater. The zinc “tannate” was precipitated at pH 4 and pH 8. Insoluble and soluble matrix antifouling paints, with different plasticizers, were formulated and tannins leached from the paints immersed in artificial seawater were determined by the Folin-Denis assay for polyphenols. The antifouling action of paints was assessed in a natural seawater environment. The results showed that the leaching rate of tannin from insoluble matrix paint decreases, reaching a constant value after 25 days of immersion. In the case of the soluble matrix paints, a lesser amount of tannin was leached, depending on the tannin and the plasticizer employed. The results in a natural sea environment are dependent on the matrix and the plasticizer employed.Centro de Investigación y Desarrollo en Tecnología de Pinturas2010info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionArticulohttp://purl.org/coar/resource_type/c_6501info:ar-repo/semantics/articuloapplication/pdf3386-3390http://sedici.unlp.edu.ar/handle/10915/94523enginfo:eu-repo/semantics/altIdentifier/doi/10.1021/ie9010518info:eu-repo/semantics/openAccesshttp://creativecommons.org/licenses/by-nc-nd/4.0/Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0)reponame:SEDICI (UNLP)instname:Universidad Nacional de La Platainstacron:UNLP2025-09-03T10:51:52Zoai:sedici.unlp.edu.ar:10915/94523Institucionalhttp://sedici.unlp.edu.ar/Universidad públicaNo correspondehttp://sedici.unlp.edu.ar/oai/snrdalira@sedici.unlp.edu.arArgentinaNo correspondeNo correspondeNo correspondeopendoar:13292025-09-03 10:51:52.245SEDICI (UNLP) - Universidad Nacional de La Platafalse |
dc.title.none.fl_str_mv |
Antifouling Paints with Zinc “Tannate” |
title |
Antifouling Paints with Zinc “Tannate” |
spellingShingle |
Antifouling Paints with Zinc “Tannate” Bellotti, Natalia Ingeniería Química Antifouling Tannin Paints |
title_short |
Antifouling Paints with Zinc “Tannate” |
title_full |
Antifouling Paints with Zinc “Tannate” |
title_fullStr |
Antifouling Paints with Zinc “Tannate” |
title_full_unstemmed |
Antifouling Paints with Zinc “Tannate” |
title_sort |
Antifouling Paints with Zinc “Tannate” |
dc.creator.none.fl_str_mv |
Bellotti, Natalia Deyá, Marta Cecilia Del Amo, Delia Beatriz Romagnoli, Roberto |
author |
Bellotti, Natalia |
author_facet |
Bellotti, Natalia Deyá, Marta Cecilia Del Amo, Delia Beatriz Romagnoli, Roberto |
author_role |
author |
author2 |
Deyá, Marta Cecilia Del Amo, Delia Beatriz Romagnoli, Roberto |
author2_role |
author author author |
dc.subject.none.fl_str_mv |
Ingeniería Química Antifouling Tannin Paints |
topic |
Ingeniería Química Antifouling Tannin Paints |
dc.description.none.fl_txt_mv |
During the past decade, the necessity of new ecofriendly antifouling pigments was established. Among these new pigments, special attention should be paid to tannin and its derivatives. Tannins are synthesized by plants as part of their defense mechanism against the attack of pathogens. The objective of this work was to study the antifouling efficiency of paints containing zinc “tannate” in artificial seawater. The zinc “tannate” was precipitated at pH 4 and pH 8. Insoluble and soluble matrix antifouling paints, with different plasticizers, were formulated and tannins leached from the paints immersed in artificial seawater were determined by the Folin-Denis assay for polyphenols. The antifouling action of paints was assessed in a natural seawater environment. The results showed that the leaching rate of tannin from insoluble matrix paint decreases, reaching a constant value after 25 days of immersion. In the case of the soluble matrix paints, a lesser amount of tannin was leached, depending on the tannin and the plasticizer employed. The results in a natural sea environment are dependent on the matrix and the plasticizer employed. Centro de Investigación y Desarrollo en Tecnología de Pinturas |
description |
During the past decade, the necessity of new ecofriendly antifouling pigments was established. Among these new pigments, special attention should be paid to tannin and its derivatives. Tannins are synthesized by plants as part of their defense mechanism against the attack of pathogens. The objective of this work was to study the antifouling efficiency of paints containing zinc “tannate” in artificial seawater. The zinc “tannate” was precipitated at pH 4 and pH 8. Insoluble and soluble matrix antifouling paints, with different plasticizers, were formulated and tannins leached from the paints immersed in artificial seawater were determined by the Folin-Denis assay for polyphenols. The antifouling action of paints was assessed in a natural seawater environment. The results showed that the leaching rate of tannin from insoluble matrix paint decreases, reaching a constant value after 25 days of immersion. In the case of the soluble matrix paints, a lesser amount of tannin was leached, depending on the tannin and the plasticizer employed. The results in a natural sea environment are dependent on the matrix and the plasticizer employed. |
publishDate |
2010 |
dc.date.none.fl_str_mv |
2010 |
dc.type.none.fl_str_mv |
info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion Articulo http://purl.org/coar/resource_type/c_6501 info:ar-repo/semantics/articulo |
format |
article |
status_str |
publishedVersion |
dc.identifier.none.fl_str_mv |
http://sedici.unlp.edu.ar/handle/10915/94523 |
url |
http://sedici.unlp.edu.ar/handle/10915/94523 |
dc.language.none.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
info:eu-repo/semantics/altIdentifier/doi/10.1021/ie9010518 |
dc.rights.none.fl_str_mv |
info:eu-repo/semantics/openAccess http://creativecommons.org/licenses/by-nc-nd/4.0/ Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0) |
eu_rights_str_mv |
openAccess |
rights_invalid_str_mv |
http://creativecommons.org/licenses/by-nc-nd/4.0/ Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0) |
dc.format.none.fl_str_mv |
application/pdf 3386-3390 |
dc.source.none.fl_str_mv |
reponame:SEDICI (UNLP) instname:Universidad Nacional de La Plata instacron:UNLP |
reponame_str |
SEDICI (UNLP) |
collection |
SEDICI (UNLP) |
instname_str |
Universidad Nacional de La Plata |
instacron_str |
UNLP |
institution |
UNLP |
repository.name.fl_str_mv |
SEDICI (UNLP) - Universidad Nacional de La Plata |
repository.mail.fl_str_mv |
alira@sedici.unlp.edu.ar |
_version_ |
1842260399809888256 |
score |
13.13397 |