The electrochemistry of gold in acid aqueous solutions containing chloride ions

Autores
Herrera Gallego, J.; Castellano, Carlos E.; Calandra, Alfredo J.; Arvia, Alejandro Jorge
Año de publicación
1975
Idioma
inglés
Tipo de recurso
artículo
Estado
versión publicada
Descripción
Results obtained with differently prepared gold electrodes in acid solutions containing chloride ion at temperatures ranging from 22 to 65°C are reported. Potentiostatic techniques and rotating disc electrodes were employed. The anodic dissolution, the onset of passivity and the cathodic deposition of the metal are investigated under different experimental conditions. The anodic dissolution of Au is discussed in terms of possible reaction mechanisms involving the participation of different adsorbed species. The onset of passivation is related to the depletion of chloride ion at the reaction interface. The experimental voltammograms can be reporduced by means of an equation which considers the diffusion of chloride ion, the activation polarization related to the dissolution of Au and the establishment of passivity.
Instituto de Investigaciones Fisicoquímicas Teóricas y Aplicadas
Facultad de Ciencias Exactas
Materia
Ciencias Exactas
Química
Electroquímica
Oro
Cloro
Electrodos
Acido
Discos Rotatorios
Nivel de accesibilidad
acceso abierto
Condiciones de uso
http://creativecommons.org/licenses/by-nc-sa/4.0/
Repositorio
SEDICI (UNLP)
Institución
Universidad Nacional de La Plata
OAI Identificador
oai:sedici.unlp.edu.ar:10915/80375

id SEDICI_3950c58cf3b8278dcdda09aed22a90e3
oai_identifier_str oai:sedici.unlp.edu.ar:10915/80375
network_acronym_str SEDICI
repository_id_str 1329
network_name_str SEDICI (UNLP)
spelling The electrochemistry of gold in acid aqueous solutions containing chloride ionsHerrera Gallego, J.Castellano, Carlos E.Calandra, Alfredo J.Arvia, Alejandro JorgeCiencias ExactasQuímicaElectroquímicaOroCloroElectrodosAcidoDiscos RotatoriosResults obtained with differently prepared gold electrodes in acid solutions containing chloride ion at temperatures ranging from 22 to 65°C are reported. Potentiostatic techniques and rotating disc electrodes were employed. The anodic dissolution, the onset of passivity and the cathodic deposition of the metal are investigated under different experimental conditions. The anodic dissolution of Au is discussed in terms of possible reaction mechanisms involving the participation of different adsorbed species. The onset of passivation is related to the depletion of chloride ion at the reaction interface. The experimental voltammograms can be reporduced by means of an equation which considers the diffusion of chloride ion, the activation polarization related to the dissolution of Au and the establishment of passivity.Instituto de Investigaciones Fisicoquímicas Teóricas y AplicadasFacultad de Ciencias Exactas1975-12-25info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionArticulohttp://purl.org/coar/resource_type/c_6501info:ar-repo/semantics/articuloapplication/pdf207-230http://sedici.unlp.edu.ar/handle/10915/80375enginfo:eu-repo/semantics/altIdentifier/issn/0022-0728info:eu-repo/semantics/altIdentifier/doi/10.1016/S0022-0728(75)80004-0info:eu-repo/semantics/openAccesshttp://creativecommons.org/licenses/by-nc-sa/4.0/Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International (CC BY-NC-SA 4.0)reponame:SEDICI (UNLP)instname:Universidad Nacional de La Platainstacron:UNLP2025-09-03T10:47:03Zoai:sedici.unlp.edu.ar:10915/80375Institucionalhttp://sedici.unlp.edu.ar/Universidad públicaNo correspondehttp://sedici.unlp.edu.ar/oai/snrdalira@sedici.unlp.edu.arArgentinaNo correspondeNo correspondeNo correspondeopendoar:13292025-09-03 10:47:03.429SEDICI (UNLP) - Universidad Nacional de La Platafalse
dc.title.none.fl_str_mv The electrochemistry of gold in acid aqueous solutions containing chloride ions
title The electrochemistry of gold in acid aqueous solutions containing chloride ions
spellingShingle The electrochemistry of gold in acid aqueous solutions containing chloride ions
Herrera Gallego, J.
Ciencias Exactas
Química
Electroquímica
Oro
Cloro
Electrodos
Acido
Discos Rotatorios
title_short The electrochemistry of gold in acid aqueous solutions containing chloride ions
title_full The electrochemistry of gold in acid aqueous solutions containing chloride ions
title_fullStr The electrochemistry of gold in acid aqueous solutions containing chloride ions
title_full_unstemmed The electrochemistry of gold in acid aqueous solutions containing chloride ions
title_sort The electrochemistry of gold in acid aqueous solutions containing chloride ions
dc.creator.none.fl_str_mv Herrera Gallego, J.
Castellano, Carlos E.
Calandra, Alfredo J.
Arvia, Alejandro Jorge
author Herrera Gallego, J.
author_facet Herrera Gallego, J.
Castellano, Carlos E.
Calandra, Alfredo J.
Arvia, Alejandro Jorge
author_role author
author2 Castellano, Carlos E.
Calandra, Alfredo J.
Arvia, Alejandro Jorge
author2_role author
author
author
dc.subject.none.fl_str_mv Ciencias Exactas
Química
Electroquímica
Oro
Cloro
Electrodos
Acido
Discos Rotatorios
topic Ciencias Exactas
Química
Electroquímica
Oro
Cloro
Electrodos
Acido
Discos Rotatorios
dc.description.none.fl_txt_mv Results obtained with differently prepared gold electrodes in acid solutions containing chloride ion at temperatures ranging from 22 to 65°C are reported. Potentiostatic techniques and rotating disc electrodes were employed. The anodic dissolution, the onset of passivity and the cathodic deposition of the metal are investigated under different experimental conditions. The anodic dissolution of Au is discussed in terms of possible reaction mechanisms involving the participation of different adsorbed species. The onset of passivation is related to the depletion of chloride ion at the reaction interface. The experimental voltammograms can be reporduced by means of an equation which considers the diffusion of chloride ion, the activation polarization related to the dissolution of Au and the establishment of passivity.
Instituto de Investigaciones Fisicoquímicas Teóricas y Aplicadas
Facultad de Ciencias Exactas
description Results obtained with differently prepared gold electrodes in acid solutions containing chloride ion at temperatures ranging from 22 to 65°C are reported. Potentiostatic techniques and rotating disc electrodes were employed. The anodic dissolution, the onset of passivity and the cathodic deposition of the metal are investigated under different experimental conditions. The anodic dissolution of Au is discussed in terms of possible reaction mechanisms involving the participation of different adsorbed species. The onset of passivation is related to the depletion of chloride ion at the reaction interface. The experimental voltammograms can be reporduced by means of an equation which considers the diffusion of chloride ion, the activation polarization related to the dissolution of Au and the establishment of passivity.
publishDate 1975
dc.date.none.fl_str_mv 1975-12-25
dc.type.none.fl_str_mv info:eu-repo/semantics/article
info:eu-repo/semantics/publishedVersion
Articulo
http://purl.org/coar/resource_type/c_6501
info:ar-repo/semantics/articulo
format article
status_str publishedVersion
dc.identifier.none.fl_str_mv http://sedici.unlp.edu.ar/handle/10915/80375
url http://sedici.unlp.edu.ar/handle/10915/80375
dc.language.none.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv info:eu-repo/semantics/altIdentifier/issn/0022-0728
info:eu-repo/semantics/altIdentifier/doi/10.1016/S0022-0728(75)80004-0
dc.rights.none.fl_str_mv info:eu-repo/semantics/openAccess
http://creativecommons.org/licenses/by-nc-sa/4.0/
Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International (CC BY-NC-SA 4.0)
eu_rights_str_mv openAccess
rights_invalid_str_mv http://creativecommons.org/licenses/by-nc-sa/4.0/
Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International (CC BY-NC-SA 4.0)
dc.format.none.fl_str_mv application/pdf
207-230
dc.source.none.fl_str_mv reponame:SEDICI (UNLP)
instname:Universidad Nacional de La Plata
instacron:UNLP
reponame_str SEDICI (UNLP)
collection SEDICI (UNLP)
instname_str Universidad Nacional de La Plata
instacron_str UNLP
institution UNLP
repository.name.fl_str_mv SEDICI (UNLP) - Universidad Nacional de La Plata
repository.mail.fl_str_mv alira@sedici.unlp.edu.ar
_version_ 1842260342804054016
score 13.13397