Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts

Autores
Canavese, Sergio Alberto; Finelli, Zunilda Rosa; Busto, Mariana; Benitez, Viviana Monica; Vera, Carlos Roman; Yori, Juan Carlos
Año de publicación
2010
Idioma
inglés
Tipo de recurso
artículo
Estado
versión publicada
Descripción
WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of Brőnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.
Fil: Canavese, Sergio Alberto. Universidad Nacional del Litoral; Argentina
Fil: Finelli, Zunilda Rosa. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Busto, Mariana. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Benitez, Viviana Monica. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Vera, Carlos Roman. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Yori, Juan Carlos. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Materia
POISONING
ISOMERIZATION
TUNGSTEN
PALLADIUM
Nivel de accesibilidad
acceso abierto
Condiciones de uso
https://creativecommons.org/licenses/by-nc-sa/2.5/ar/
Repositorio
CONICET Digital (CONICET)
Institución
Consejo Nacional de Investigaciones Científicas y Técnicas
OAI Identificador
oai:ri.conicet.gov.ar:11336/101233

id CONICETDig_d7933ab1bf1f2fe9f0441d5e4e598625
oai_identifier_str oai:ri.conicet.gov.ar:11336/101233
network_acronym_str CONICETDig
repository_id_str 3498
network_name_str CONICET Digital (CONICET)
spelling Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalystsCanavese, Sergio AlbertoFinelli, Zunilda RosaBusto, MarianaBenitez, Viviana MonicaVera, Carlos RomanYori, Juan CarlosPOISONINGISOMERIZATIONTUNGSTENPALLADIUMhttps://purl.org/becyt/ford/2.4https://purl.org/becyt/ford/2WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of Brőnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.Fil: Canavese, Sergio Alberto. Universidad Nacional del Litoral; ArgentinaFil: Finelli, Zunilda Rosa. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; ArgentinaFil: Busto, Mariana. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; ArgentinaFil: Benitez, Viviana Monica. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; ArgentinaFil: Vera, Carlos Roman. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; ArgentinaFil: Yori, Juan Carlos. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; ArgentinaSociedade Brasileira de Química2010-02info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionhttp://purl.org/coar/resource_type/c_6501info:ar-repo/semantics/articuloapplication/pdfapplication/pdfapplication/pdfapplication/pdfapplication/pdfapplication/pdfhttp://hdl.handle.net/11336/101233Canavese, Sergio Alberto; Finelli, Zunilda Rosa; Busto, Mariana; Benitez, Viviana Monica; Vera, Carlos Roman; et al.; Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts; Sociedade Brasileira de Química; Química Nova; 33; 2-2010; 508-5130100-40421678-7064CONICET DigitalCONICETenginfo:eu-repo/semantics/altIdentifier/url/http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422010000300003&lng=en&nrm=isoinfo:eu-repo/semantics/altIdentifier/url/http://quimicanova.sbq.org.br/audiencia_pdf.asp?aid2=4987&nomeArquivo=Vol33No3_508_02-AR08619.pdfinfo:eu-repo/semantics/openAccesshttps://creativecommons.org/licenses/by-nc-sa/2.5/ar/reponame:CONICET Digital (CONICET)instname:Consejo Nacional de Investigaciones Científicas y Técnicas2025-09-03T09:59:01Zoai:ri.conicet.gov.ar:11336/101233instacron:CONICETInstitucionalhttp://ri.conicet.gov.ar/Organismo científico-tecnológicoNo correspondehttp://ri.conicet.gov.ar/oai/requestdasensio@conicet.gov.ar; lcarlino@conicet.gov.arArgentinaNo correspondeNo correspondeNo correspondeopendoar:34982025-09-03 09:59:01.919CONICET Digital (CONICET) - Consejo Nacional de Investigaciones Científicas y Técnicasfalse
dc.title.none.fl_str_mv Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
title Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
spellingShingle Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
Canavese, Sergio Alberto
POISONING
ISOMERIZATION
TUNGSTEN
PALLADIUM
title_short Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
title_full Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
title_fullStr Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
title_full_unstemmed Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
title_sort Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
dc.creator.none.fl_str_mv Canavese, Sergio Alberto
Finelli, Zunilda Rosa
Busto, Mariana
Benitez, Viviana Monica
Vera, Carlos Roman
Yori, Juan Carlos
author Canavese, Sergio Alberto
author_facet Canavese, Sergio Alberto
Finelli, Zunilda Rosa
Busto, Mariana
Benitez, Viviana Monica
Vera, Carlos Roman
Yori, Juan Carlos
author_role author
author2 Finelli, Zunilda Rosa
Busto, Mariana
Benitez, Viviana Monica
Vera, Carlos Roman
Yori, Juan Carlos
author2_role author
author
author
author
author
dc.subject.none.fl_str_mv POISONING
ISOMERIZATION
TUNGSTEN
PALLADIUM
topic POISONING
ISOMERIZATION
TUNGSTEN
PALLADIUM
purl_subject.fl_str_mv https://purl.org/becyt/ford/2.4
https://purl.org/becyt/ford/2
dc.description.none.fl_txt_mv WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of Brőnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.
Fil: Canavese, Sergio Alberto. Universidad Nacional del Litoral; Argentina
Fil: Finelli, Zunilda Rosa. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Busto, Mariana. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Benitez, Viviana Monica. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Vera, Carlos Roman. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
Fil: Yori, Juan Carlos. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Santa Fe. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera". Universidad Nacional del Litoral. Instituto de Investigaciones en Catálisis y Petroquímica "Ing. José Miguel Parera"; Argentina
description WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of Brőnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.
publishDate 2010
dc.date.none.fl_str_mv 2010-02
dc.type.none.fl_str_mv info:eu-repo/semantics/article
info:eu-repo/semantics/publishedVersion
http://purl.org/coar/resource_type/c_6501
info:ar-repo/semantics/articulo
format article
status_str publishedVersion
dc.identifier.none.fl_str_mv http://hdl.handle.net/11336/101233
Canavese, Sergio Alberto; Finelli, Zunilda Rosa; Busto, Mariana; Benitez, Viviana Monica; Vera, Carlos Roman; et al.; Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts; Sociedade Brasileira de Química; Química Nova; 33; 2-2010; 508-513
0100-4042
1678-7064
CONICET Digital
CONICET
url http://hdl.handle.net/11336/101233
identifier_str_mv Canavese, Sergio Alberto; Finelli, Zunilda Rosa; Busto, Mariana; Benitez, Viviana Monica; Vera, Carlos Roman; et al.; Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts; Sociedade Brasileira de Química; Química Nova; 33; 2-2010; 508-513
0100-4042
1678-7064
CONICET Digital
CONICET
dc.language.none.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv info:eu-repo/semantics/altIdentifier/url/http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422010000300003&lng=en&nrm=iso
info:eu-repo/semantics/altIdentifier/url/http://quimicanova.sbq.org.br/audiencia_pdf.asp?aid2=4987&nomeArquivo=Vol33No3_508_02-AR08619.pdf
dc.rights.none.fl_str_mv info:eu-repo/semantics/openAccess
https://creativecommons.org/licenses/by-nc-sa/2.5/ar/
eu_rights_str_mv openAccess
rights_invalid_str_mv https://creativecommons.org/licenses/by-nc-sa/2.5/ar/
dc.format.none.fl_str_mv application/pdf
application/pdf
application/pdf
application/pdf
application/pdf
application/pdf
dc.publisher.none.fl_str_mv Sociedade Brasileira de Química
publisher.none.fl_str_mv Sociedade Brasileira de Química
dc.source.none.fl_str_mv reponame:CONICET Digital (CONICET)
instname:Consejo Nacional de Investigaciones Científicas y Técnicas
reponame_str CONICET Digital (CONICET)
collection CONICET Digital (CONICET)
instname_str Consejo Nacional de Investigaciones Científicas y Técnicas
repository.name.fl_str_mv CONICET Digital (CONICET) - Consejo Nacional de Investigaciones Científicas y Técnicas
repository.mail.fl_str_mv dasensio@conicet.gov.ar; lcarlino@conicet.gov.ar
_version_ 1842269556428505088
score 13.13397